Ferrite is the cheapest magnetic material and has a high corrosion resistance making coating unnecessary. This magnetic material is hard and fragile and must be processed with diamond, preferably when it is not in a magnetic state. Because it might shrink during the sinter process a tolerance of ± 2 % should be taken into account when determining t1